INFO & QUOTE REQUESTS: info@saphonyx.be

M.R.O. range

Passivation after rust removal

After deoxidation, the surface can become extremely susceptible to corrosion, depending on the metal: it must be passivated or given corrosion protection, depending on the next treatment and how soon it will be carried out.

  • Next step: apply corrosion protection suited to the storage period.

Steel and cast iron

BONDERITE S-FN 7400

Non-foaming aqueous corrosion protection with organic inhibitors and no mineral oil: for passivation of steel and cast iron (formerly P3-PREVOX 7400).

Dip or spray: 5 to 20 g/l for steel, 15 to 30 g/l for cast iron, at 15 to 80 °C for more than 30 s; short-term protection (up to one week).

Technical data sheet (PDF) →

BONDERITE S-FN 5081

Aqueous temporary corrosion protection, free of mineral oil, for longer periods of intermediate storage indoors (formerly P3-PREVOX 5081).

Immersion or spray: 10 to 30 g/l at 20 to 80 °C for 0.5 to 3 min.

Technical data sheet (PDF) →

BONDERITE S-FN T320

Oil-free alkaline passivation agent: converts iron salts remaining after acid pickling into salts that can be removed, leaving a uniform surface (formerly P3-T 320).

Immersion or spray: for iron salt removal, 20 to 40 g/l at 20 to 60 °C for 1 to 5 min; for passivation, 2 to 5 g/l at 65 °C.

Technical data sheet in English (PDF) →

Stainless steel

BONDERITE C-IC 18010 (LIQUID / PASTE)

Nitric acid-free pickling agent for stainless steel: removes weld oxides and rust and passivates the stainless steel (ASTM A967).

Use undiluted at room temperature for 20 min to several hours: apply LIQUID by immersion and PASTE by brush; rinse thoroughly.

Request the technical data sheet →

After ultrasonic cleaning

TICKOPUR KS 1

All-purpose corrosion protection for ferrous metals after cleaning with TICKOPUR and rinsing; solvent-free and leaves no greasy film; for indoor storage.

0.5 to 2%; neutral (pH 7.4 at 1%).

Request the technical data sheet →

See also:
Corrosion protection after passivation →
Rust removal in maintenance (by oxide type) →
Passivation after pickling →
Surface treatment, “Corrosion protection” →

Need advice?

Tell us what you need to treat, on which substrate and with what equipment: we will recommend a product and method and send you the technical data sheets and safety data sheets or a quotation.