INFO & QUOTE REQUESTS: info@saphonyx.be

T.S.M. range

Stainless steel treatment

After welding, heat treatment, grinding or machining, stainless steel has oxides or ferrous particles on its surface that impair its corrosion resistance.

We offer products for degreasing, descaling, pickling and brightening stainless steel.

  • Typical immersion process: alkaline degreasing, rinse, pickling, rinse, passivation, rinse, drying (contact us about passivation).
  • BONDERITE C-IC 18010 is free from nitric acid; it is labelled as corrosive but not as toxic.
  • The C-IC STA / C-AD STB brightening process causes neither hydrogen embrittlement nor intergranular corrosion.

Recommended products

BONDERITE C-AK L-95

Strongly alkaline, phosphate-free liquid degreaser for use with a surfactant additive

Stainless steel: 50 to 100 g/l, 50 to 90 °C, 5 to 15 min; use BONDERITE C-AD 0470 as the additive for immersion or C-AD 2000 for spray application

Technical data sheet (PDF) →

BONDERITE C-AK 4181 L AERO

Strongly alkaline degreaser and descaler, safe for martensitic and austenitic stainless steels

Spray or immersion; descaling: 30 g/l; degreasing: 10 to 20 g/l, 50 to 80 °C

Technical data sheet (PDF) →

BONDERITE C-IC 4104 AERO

Additive for nitric acid baths: descaling and pickling of stainless steels and refractory alloys (formerly TURCO NITRADD)

Immersion; bath composition adjusted to suit the alloy

Technical data sheet in English (PDF) →

BONDERITE C-IC 18010 LIQUID

Nitric acid-free pickling agent for stainless steels: removes weld oxides and ferrous contamination

Use undiluted by immersion, after degreasing if necessary; immerse for 20 min to several hours, then rinse thoroughly

Technical data sheet (PDF) →

BONDERITE C-IC 18010 PASTE

Gel version of the C-IC 18010 pickling agent for localised treatment of welds and surfaces

Apply a layer approximately 2 mm thick with a brush, roller or spatula; leave for 20 min to several hours

Technical data sheet (PDF) →

BONDERITE C-IC STA + C-AD STB

Patented fluoride-free process for chemical brightening of stainless steels (formerly NOVABRITE STA / STB)

Austenitic stainless steels and nickel-based alloys; immersion in 96% STA + 4% STB (by weight), 78 ± 2 °C, 3 to 8 min

Request the technical data sheet →

See also:
Surface treatment page, “Decorative treatment of metals” →
Brightening and treatment of stainless steel →

Need advice?

Tell us what you need to treat, on which substrate and with what equipment: we will recommend a product and method and send you the technical data sheets and safety data sheets or a quotation.