Crystalline phosphating

Crystalline phosphating forms a zinc or manganese phosphate layer that provides a base for paint adhesion, improves corrosion protection and, with an oil or grease finish, reduces friction between mechanical parts.

BONDERITE processes are applied by immersion or spray before painting, cathodic electrocoating or oiling.

  • Typical zinc phosphating sequence: surface cleaning and activation, phosphating, rinsing and post-passivation.
  • Manganese phosphating: a grey to black layer that retains oil and limits galling during running-in.
  • Phosphate-free alternative to zinc phosphating: BONDERITE M-NT 1200 (see Multimetal conversion coating).

Recommended products

BONDERITE M-ZN 2722 E6

Nickel-free, nitrite-accelerated bi-cation zinc phosphating; crystalline layer of 2 to 2.8 g/m², suitable for use before cathodic electrocoating (formerly GRANODINE 2722 E-6 M)

Steel, galvanized steel and Zn/Ni-coated steels; spray, 50 to 55 °C, 60 to 180 s

Technical data sheet (PDF) →

BONDERITE M-ZN 45

Crystalline phosphating by dipping before painting: microcrystalline layer of zinc and iron phosphates (formerly GRANODINE 45)

Ferrous surfaces; immersion, 4% + 1% BONDERITE M-AD ZN-2, 70 to 85 °C, 6 to 15 min

Technical data sheet (PDF) →

BONDERITE M-ZN 220

Microcrystalline zinc phosphating by immersion, intended for subsequent application of a rust-preventive oil, grease or wax (formerly GRANODINE 220)

Cast iron, plain carbon steels and low-alloy steels; 5 to 8 L + 2 L of BONDERITE M-AD CA-1 per 100 L, 65 to 70 °C, 5 to 10 min

Technical data sheet (PDF) →

BONDERITE M-MN 2252

Manganese phosphating of steel and cast iron friction components; a single product for bath make-up and maintenance (formerly NOVAPHOS M 2252)

Immersion (barrel, basket or rack), 80 to 100 L per 1,000 L, 95 to 98 °C, 5 to 15 min

Technical data sheet (PDF) →

BONDERITE M-AC 50 CF

Grain refiner for use before crystalline zinc phosphating, suitable for bath make-up with industrial water (formerly FIXODINE 50 CF)

By immersion or in the second rinse after degreasing, immediately before phosphating

Technical data sheet (PDF) →

BONDERITE M-AC TG-2 / M-AC TG-2 B

Two-component grain refiner for use before manganese phosphating: a fine, homogeneous layer with a uniform black appearance (formerly FIXODINE TG 2A / TG 2B)

Essential after strongly alkaline degreasing or acid pickling

Request the technical data sheet →

BONDERITE M-PT 54 NC

Chrome-free inorganic passivating post-rinse for zinc and iron phosphate layers (formerly DEOXYLYTE 54 NC)

Spray or immersion, 2.5 ml/L, pH 4 to 4.5 (adjusted with M-AD 80L), 20 to 55 °C, 15 to 90 s

Technical data sheet (PDF) →

BONDERITE M-NT 1455T

Chrome-free passivation after amorphous phosphating or crystalline zinc phosphating; ELV and RoHS compliant (formerly GRANODINE 1455 T)

Immersion or spray, 2 to 10 ml/L (typically 5 ml/L), 20 to 40 °C, 20 to 60 s

Technical data sheet (PDF) →

See also:
Surface treatment page, “Conversion coating” and “Seal / Post-rinse (chrome-free)” →
Multimetal conversion coating →

Need advice?

Tell us what you need to treat, on which substrate and with what equipment: we will recommend a product and method and send you the technical data sheets and safety data sheets or a quotation.