Multimetal conversion coating

BONDERITE M-NT conversion coatings replace iron or zinc phosphating before painting: they treat steel, galvanized steel and aluminium on the same line, with little or no phosphate and often fewer stages.

Saphonyx manages process baths on conversion coating lines and provides support for small lines and new technologies.

  • APNR (Adhesion Promoter No Rinse): applying a fine mist of adhesion promoter at the end of pretreatment retains the footprint of a 3-stage tunnel while providing the performance guarantees of a 5-stage tunnel.
  • On-site touch-ups: use BONDERITE M-NT 1455 WIPES without dismantling or rinsing.

Recommended products

BONDERITE M-NT 1200

Phosphate-free conversion coating designed to replace crystalline zinc phosphating; eliminates grain refinement and passivation (formerly TECTALIS 1200)

Steel, electrogalvanized steel, galvanized steel, aluminium; spray application in existing installations, 30 g/l at bath make-up, 20 to 40 °C, 20 to 180 s

Technical data sheet (PDF) →

BONDERITE M-NT 40043

Conversion coating based on zirconium salts that replaces amorphous phosphating and has a much lower phosphate content

Immersion or spray, 10 to 30 ml/l; 20 to 25 °C for conversion coating alone, 40 to 60 °C for combined degreasing and conversion coating

Technical data sheet (PDF) →

BONDERITE M-NT 1

Phosphate-free “nanoceramic” conversion coating that replaces amorphous phosphating and eliminates passivation (formerly BONDERITE NT 1)

Steel, electrogalvanized steel, galvanized steel, aluminium; immersion or spray, 30 to 50 ml/l, 20 to 30 °C, 20 to 120 s

Technical data sheet (PDF) →

BONDERITE M-NT 20120

Conversion coating free of phosphates, VOCs and toxic heavy metals; limits “flash rust” during line stoppages

Steel, galvanized steel, aluminium; spray or immersion without heating, 1 to 3.5%, 20 to 50 °C, 20 to 120 s

Technical data sheet (PDF) →

BONDERITE M-NT 30002

Phosphate-free conversion coating based on trivalent chromium and zirconium, suitable for zinc-coated substrates

Steel, galvanized steel, aluminium; spray or immersion, 3% at bath make-up, 20 to 35 °C, 30 to 120 s

Technical data sheet (PDF) →

BONDERITE M-NT 50001

No-rinse thin-film conversion coating (APNR process) for lines with fewer than 5 stages

Steel, galvanized steel, aluminium; spray application after degreasing using the APNR equipment, 0.2 to 1%, room temperature, 5 to 60 s

Technical data sheet in English (PDF) →

BONDERITE M-NT 1455 WIPES

Wipes pre-impregnated with a chrome-free conversion coating for touch-ups without dismantling or rinsing (formerly GRANODINE 1455 WIPES)

Aluminium, zinc, steel, electrogalvanized steel and galvanized steel; apply by dabbing or wiping, undiluted, 20 to 30 °C, 30 to 60 s

Request the technical data sheet →

See also:
Surface treatment page, “Multimetal conversion coatings” →
BONDERITE M-NT 1455 WIPES →
Iron phosphating →
Crystalline phosphating →