Iron phosphating
Iron (or amorphous) phosphating forms a non-crystalline layer of iron phosphate on steel that improves paint adhesion and corrosion protection.
Depending on the product, iron phosphating is carried out in a single step (combined degreasing and phosphating) or after a separate degreasing step, by spray, by immersion or with a high-pressure lance. Saphonyx provides support in particular for small phosphating lines.
- Typical sequence in a 3-stage tunnel: combined degreasing and phosphating, rinse, passivation; sequences with 4 or 5 stages are also possible.
- After the final rinse, the parts are dried and then painted without delay.
- Phosphate-free alternatives: BONDERITE M-NT 40043, M-NT 1 and M-NT 20120 (see Multimetal conversion coating).
Recommended products
BONDERITE M-FE HP
Liquid degreasing and phosphating agent for use with high-pressure equipment on large parts that cannot be treated in a tunnel (formerly NOVAPHOS F HP)
8 to 15 ml/l at the lance outlet, 60 to 90 °C, 20 to 80 bar; coating weight of 0.2 to 0.7 g/m²
BONDERITE M-FE 30A
Amorphous phosphating with a high coating weight for ferrous metals, with a detergent additive (formerly NOVAPHOS F 30 A)
Spray tunnel, 10 to 25 ml/l + 1.5 to 3 ml/l of additive, 30 to 55 °C, 90 to 180 s; coating weight of 0.5 to 1 g/m²
BONDERITE M-FE F-813
Amorphous phosphating with a high coating weight for ferrous metals, with a detergent additive (formerly DURIDINE F 813 CF)
Spray tunnel, 12 to 25 ml/l + 1.5 to 3 ml/l of additive, 30 to 55 °C, 90 to 180 s
BONDERITE M-FE F-814
Single-step degreasing and amorphous phosphating of steel, usable at temperatures as low as 25 °C (formerly DURIDINE F 814 CF)
Three- or four-stage spray tunnel; 2% at 35–40 °C for 3 min, up to 4% for 1 min
BONDERITE M-FE 1070
Multimetal degreasing and phosphating: steel, light alloys, galvanized steel, zinc plated steel (formerly DURIDINE 1070)
Spray for 90 s to 3 min or immerse for 3 to 8 min; 3 to 6% by volume, 40 to 65 °C
BONDERITE M-PT 98 NC
Chrome-free passivation after amorphous phosphating: improves corrosion protection and paint adhesion (formerly DEOXYLYTE 98 NC)
Immersion or spray, 0.5 to 2 ml/l (0.2 to 1 ml/l in deionized water), 20 to 40 °C, 20 to 60 s
See also:
Surface treatment page, “Conversion coating” and “Alternatives to iron phosphating” →