INFO & QUOTE REQUESTS: info@saphonyx.be

T.S.M. range

Removal of oxides and the primary oxidation layer (POL)

Removal of oxides and the POL (Primary Oxidation Layer): degreasing and deoxidation processes for copper alloys (tombac, bronze, beryllium copper, brass, nickel silver).

For steel, cast iron, galvanized steel, stainless steel, magnesium, titanium and aluminium, see the linked pages. Operating conditions are indicative: refer to the technical data sheet (TDS).

Processes by copper alloy

  • Tombac and brass: BONDERITE C-IC AS at 50% (hydrochloric acid-based), 50 °C, 30 min, rinse with deionized (DI) water, then undiluted C-IC YMD (based on phosphoric, sulphuric, nitric and hydrochloric acids), at room temperature, 1 min, rinse with DI water at 25 °C.
  • Beryllium copper: same process using C-IC AS followed by C-IC YMD; alternatives: C-IC 62 at 20% (based on phosphoric and nitric acids), 40 °C, 15 min, or C-IC SC-58 CF at 40 g/l (sulphamic acid-based), 50 °C, 15 min.
  • Bronze: C-MC 181 at 20% (based on phosphoric and nitric acids) with 10 ml/l of fluorinated additive, 50 °C, 15 min; or C-IC 62 at 20 or 30%, 40 °C, 15 min.
  • Nickel silver: process using C-IC AS followed by C-IC YMD; or C-MC 181 at 20%, 50 °C, 15 min, with or without 10 ml/l of fluorinated additive.

Copper alloys: degreasing

BONDERITE C-AK T308

Powder degreaser for steel surfaces heavily contaminated with oils, greases or drawing and wire-drawing soaps (stearates) (formerly P3-T 308)

Immersion; 5 to 20 g/l, 40 to 80 °C, 1 to 15 min

Technical data sheet (PDF) →

BONDERITE C-NE N-3

Near-neutral liquid degreaser for metal surfaces; when used with ultrasonics, removes polishing compounds from aluminium, zamak and copper alloys (formerly LUMINOL N°3)

Immersion or ultrasonic cleaning; 30 to 60 ml/l, 60 to 80 °C; 3 to 10 min by immersion, 1 to 4 min with ultrasonics

Technical data sheet (PDF) →

BONDERITE C-NE 6523-1

Liquid cleaner for stainless steel, steel, copper, aluminium and zinc alloys: removes cutting, stamping and wire-drawing fluids, grinding residues and polishing compounds; leaves a hydrophobic film that speeds up drying and passivates steel (formerly P3-VR 6523-1)

Immersion, with or without ultrasonics; 20 to 80 g/l, 40 to 90 °C; 5 to 15 min (30 to 120 s with ultrasonics)

Technical data sheet (PDF) →

TICKOPUR TR 7

Weakly alkaline all-purpose cleaner: removes drilling, grinding, polishing and lapping residues, oils, greases, wax, pigments, fluxes and brazing pastes; for all types of steel, glass, ceramics, plastics and rubber

0.1 to 5%, 20 to 60 °C, 1 to 10 min

Request the technical data sheet →

Copper alloys: deoxidation

BONDERITE C-IC YMD

Single-component liquid process for chemical brightening of copper and its alloys (brasses, bronze, nickel silver, cupronickel): produces a mirror finish; provides good surface preparation for electroless or electrolytic plating (formerly NOVABRITE YMD)

Immersion; undiluted, 20 to 25 °C, 1 to 5 min

Technical data sheet (PDF) →

BONDERITE C-IC R

Liquid acid degreaser and deoxidizer: light phosphating of steel before painting, degreasing before hot-dip galvanizing, removal of white rust and mineral deposits (formerly NOVOX R)

Manual application, immersion, circulation or spray; 20 to 50%, 20 to 60 °C, 5 to 30 min

Technical data sheet (PDF) →

BONDERITE C-IC AS

Inhibited liquid acid deoxidizer: pickling, rust removal and descaling before plating, conversion coating or hot-dip galvanizing; on copper alloys, used as the first step before brightening with C-IC YMD (formerly NOVOX AS)

Immersion; 20 to 50%, 20 to 70 °C, 5 to 30 min

Technical data sheet (PDF) →

BONDERITE C-MC 181

Acid formulation for descaling stainless steel phosphating stages by circulation; used here for deoxidation of bronze and nickel silver (formerly PROGAL G 181 DR)

Descaling: 5 to 10% by spray, 10 to 20% by dipping, room temperature to 50 °C, 1 to 6 h

Technical data sheet (PDF) →

BONDERITE C-IC 62

Acid additive free from hydrofluoric acid for nitric acid baths used to pickle titanium and its alloys; also used on bronze and beryllium copper (formerly DEOXIDIZER 62)

20 to 100 ml/l, 20 to 32 °C, 10 to 20 min

Technical data sheet (PDF) →

BONDERITE C-IC SC-58 CF

Chromic acid-free deoxidizing of aluminium and its alloys by dipping or spraying, without sludge formation, before painting, spot welding, anodizing or conversion coating; also used on beryllium copper (formerly DEOXIDINE SC 58 CF)

Spray: 10 to 20 g/l, 2 to 3 min; dipping: 30 to 50 g/l, 5 to 10 min; 20 to 60 °C

Technical data sheet (PDF) →

TICKOPUR RW 77

Special weakly alkaline cleaner containing ammonia: removes resinous residues, pigments, wax, silicone oil, soot, fluxes and non-ferrous metal oxides; use with caution on light metals

5%, 20 to 60 °C, 1 to 10 min

Request the technical data sheet →

TICKOPUR J 80 U

Acid anti-tarnish deoxidizer for jewellery, religious objects, coins and precious metals; also deoxidizes brass and copper and removes sulphides; use with caution on sensitive parts and artificially oxidised finishes

1 to 5%, 20 to 60 °C; less than 30 s with ultrasonics, less than 3 min without

Request the technical data sheet →

See also:
Steel, cast iron, galvanized steel: Acid and neutral deoxidation →
Aluminium: Chrome-free deoxidizers for aluminium →
Stainless steel treatment →
Magnesium treatment →
Titanium treatment →
Decorative metal treatment →
TICKOPUR →

Need advice?