INFO & QUOTE REQUESTS: info@saphonyx.be

Surface treatment

Corrosion protection

Protect parts between operations and during storage, and limit attack by acid baths

The metalworking industry requires active corrosion protection for parts. Intermediate storage has become more frequent, and parts pass through a wider range of environments, some of them harsh. Oxidation of bare parts is mainly due to contact with oxygen in the air and fluctuations in humidity and temperature.

Henkel products cover the various types of protection needed between operations and for short- or long-term storage.

Protection methods

Corrosion protection creates a barrier against external attack using various methods:

  • wrapping in Zerust® Excor® corrosion-inhibiting film from Acobal;
  • painting;
  • protective oils and dewatering fluids (water-displacing fluids);
  • film-forming amine;
  • phosphating;
  • conversion coating;
  • electroplated coatings (zinc plating, electrogalvanizing) or hot-dip galvanizing;
  • zinc thermal spraying.

Testing corrosion protection

Standardised corrosion tests assess the performance of each method:

Test Standard
Neutral salt spray (NSS), acetic acid salt spray (AASS) or copper-accelerated acetic acid salt spray (CASS) ISO 9227
Kesternich (sulphur dioxide atmosphere) DIN 50018 / ISO 6988
Cast iron chip corrosion test DIN 51360
Resistance to liquids by immersion ISO 2812

Film-forming protection

BONDERITE S-PR 3

Oil for temporary corrosion protection (formerly P3-GEROCOR 3). Leaves an oil film of approximately 1.5 g/m². Provides 3 to 6 months of protection in covered storage

Substrates and methods: Steel, cast iron; immersion – spray gun; use neat at room temperature (15 to 30 °C) for 0.5 to 3 min; applications: protection of parts during storage and shipping

Technical data sheet (PDF) →

BONDERITE S-FN 6764

Emulsion for medium-term corrosion protection (formerly P3-PREVOX 6764). Neat oil with added corrosion inhibitors; dry or oily appearance depending on concentration

Substrates and methods: Clean steel and cast iron parts; immersion – fine spray – spray; dry appearance at 2 to 5%, oily appearance at 5 to 20%; room temperature; drying recommended; applications: temporary protection of parts for storage in an enclosed warehouse; remove with a hot solution of BONDERITE C-NE 175

Technical data sheet (PDF) →

BONDERITE S-PR 97-10

Water-emulsifiable product for temporary corrosion protection (formerly EMULPON 97-10). Designed for very soft water (as low as 1 °dH); not recommended above 20 °dH

Substrates and methods: Steel, cast iron; immersion – spray, particularly in the final stage of multistage systems; immersion: 10 to 40 g/l, spray: 10 to 30 g/l; 10 to 80 °C; 0.5 to 3 min; applications: protection of steel and cast iron for subsequent storage in an enclosed, heated warehouse

Technical data sheet (PDF) →

BONDERITE S-FN AQUASTOP

Water-repellent fluid with corrosion-inhibiting properties (formerly TURCO AQUASTOP). Displaces water from parts: no drying step is needed. The residual film provides temporary protection during indoor storage

Substrates and methods: Metal parts; does not attack metals; protects ferrous metals from oxidation; immersion (usual method) – fine spray – brush; ready to use neat; can be diluted with white spirit for a thinner film; applications: drying and protection of parts between machining operations, after alkaline degreasing, electrolytic treatment, blackening or paint stripping

Technical data sheet (PDF) →

Passivation

BONDERITE S-FN 7400

Aqueous corrosion protection product (formerly P3-PREVOX 7400). Organic corrosion inhibitors, free from mineral oil; non-foaming

Substrates and methods: Steel, cast iron (does not inhibit corrosion on light metals or other non-ferrous metals); dipping – spray – fine spray, particularly in the final zone of a tunnel; steel: 5 to 20 g/l, cast iron: 15 to 30 g/l; 15 to 80 °C; more than 30 s; applications: passivation of steel and cast iron in leak-test tanks for hollow components, cooling circuits and degreasing baths before painting

Technical data sheet (PDF) →

BONDERITE S-FN 6304

Mildly alkaline temporary protection, free from oil and amines (formerly P3-PREVOX 6304). Provides sufficient protection for storage between operations and for hydraulic testing

Substrates and methods: Metal parts; on non-ferrous metals, do not exceed the specified parameters (risk of discolouration); spray – immersion; spray: 1 to 5 g/l, immersion: 3 to 10 g/l; 20 to 60 °C; 20 to 60 s; applications: temporary protection of parts stored between operations and during hydraulic testing

Technical data sheet (PDF) →

BONDERITE S-FN 5081

Aqueous temporary corrosion protection, free from mineral oil (formerly P3-PREVOX 5081, previously S-PR 5081). Organic corrosion-inhibiting components; no troublesome foaming between 20 and 80 °C

Substrates and methods: Steel, cast iron (long contact times may discolour non-ferrous metals); immersion – spray, particularly in the final zone of a multi-zone degreasing system; 10 to 30 g/l; 20 to 80 °C; 0.5 to 3 min; applications: passivation before intermediate storage in enclosed premises; additive for leak-test water and cooling water

Technical data sheet (PDF) →

BONDERITE S-FN T320

Oil-free alkaline passivation agent (formerly P3-T 320). Converts iron salts remaining after pickling into complex salts that can be removed, leaving a uniform, bright surface.

Substrates and methods: Pickled steel, degreased and pickled sheet metal; cast iron; immersion – spray; iron salt removal: 20 to 40 g/L, 20 to 60 °C, 1 to 5 min; passivation: 2 to 5 g/L at 65 °C; Applications: Post-treatment of steel pickled in hydrochloric or sulphuric acid and final passivation before storage

Technical data sheet in English (PDF) →

VCI protection (volatile corrosion inhibitors)

ZERUST® / EXCOR® (Acobal)

Packaging with volatile corrosion inhibitors (VCI). Films, covers and bags, papers, foams, emitter capsules

Substrates and methods: Metal parts and subassemblies; packaging for storage and transport; Applications: Corrosion protection without oil or grease – see the Zerust Excor range

Full range: Zerust® Excor®: anti-corrosion packaging.

Inhibitors for acid pickling baths

Strong acids remove oxide and mill scale before subsequent stages of a production line, or are used, for example, to clean pipework during maintenance. They also attack the base metal and cause substantial metal loss; hydrogen entering the metal makes it brittle. Inhibitors reduce acid attack on the metal and prevent hydrogen embrittlement without interfering with the removal of oxide or limescale.

Saphonyx offers a range of inhibitors and additives that limit acid attack in hydrochloric, sulphuric, hydrofluoric, phosphoric, acetic, sulphamic, citric and oxalic acid pickling baths, particularly for:

  • hot-dip galvanizing;
  • electroplating;
  • deoxidation;
  • descaling with hydrochloric acid;
  • pickling steel, cast iron and galvanized steel.

Hot-dip galvanizing

Electrolytic zinc plating and phosphating

The inhibitors

BONDERITE S-AD 31A

Liquid, chloride-free pickling inhibitor (limits acid attack). For phosphoric, sulphuric, amidosulphonic, acetic, citric and formic acids. Former name: Rodine 31 A (BONDERITE S-AD 31A)

Substrates and methods: Steel, cast iron, hot-dip galvanized steel; not for use on electrogalvanized steel; 1 to 5 L per 1,000 L of bath, depending on temperature; Applications: Compatible with phosphoric, sulphuric, sulphamic, acetic, oxalic, formic and citric acids

Technical data sheet (PDF) →

BONDERITE S-AD 60 /S-AD 1600 IT

Inhibitors that limit acid attack in hydrochloric acid pickling baths. S-AD 60: low-temperature pickling (former name: Rodine 60). S-AD 1600 IT: non-foaming, for static or continuous pickling (former name: Rodine 1600 IT)

Substrates and methods: Steel, cast iron, hot-dip galvanized steel (not for use on electrogalvanized steel); S-AD 60: 0.5 to 5 kg per 1,000 L, 20 to 40 °C; S-AD 1600 IT: 0.8 to 3 kg per 1,000 L of acid, up to 100 °C; Applications: Compatible with hydrochloric acid

Request the technical data sheet →

BONDERITE S-AD 145L

Inhibitor additive for acid baths (formerly RODINE 145 L).

Intended use: corrosion inhibitor (Henkel safety data sheet 225416); contact us for compatible acids and dosage.

Request the technical data sheet →

See also:
Deoxidation, rust removal and descaling →
Phosphating →
Conversion coating: multimetal and aluminium →
Zerust® Excor®: anti-corrosion packaging →
Surface treatment: all ranges →

Need advice?