Phosphating
Iron, zinc or manganese: pretreatment before painting, corrosion protection, metal forming and friction applications
Phosphating is a conversion coating process. It provides a key for organic coatings, improves corrosion protection and retains lubricant for metal forming and friction applications.
Our processes meet the requirements of the automotive, steelmaking, metalworking, aerospace, domestic appliance and packaging industries. Patented and available worldwide, they incorporate the latest advances in environmental protection, hygiene, safety and productivity.
Applications
Before painting
- “amorphous” iron phosphating: dipping, spray or high-pressure application; multimetal; low or high coating weight; inorganic or organic accelerator; one- or two-component;
- microcrystalline phosphating: dipping or spray; multimetal; bi- or tri-cation; nitrite-free inorganic accelerator; low-nickel or nickel-free.
Corrosion protection
Before an oil or dry finish: processes and finishes that comply with ISO standards and automotive industry requirements.
Cold forming
Drawing, wire drawing, extrusion and cold heading of steel, stainless steel and aluminium.
Friction
- low- or high-temperature manganese phosphating (75 °C and 95 °C);
- for mechanical parts subject to friction;
- new nickel-free range.
Zinc phosphating
Unlike chromium or zirconium/titanium conversion coating, which forms an amorphous layer, phosphating forms a dense layer of zinc phosphate crystals. Each crystal provides an anchor point for paint or varnish.
On an assembled car, phosphating improves paint adhesion and therefore corrosion resistance. The process works on different metals: this is important because almost all manufacturers combine steel and aluminium, and the paint must look the same on both.
- light to dark grey appearance;
- good base for paint.
Zinc phosphate crystals: immersion
Zinc phosphate crystals: spray
Phosphating line
Manganese phosphating
A manganese phosphate coating is thicker than an iron or zinc phosphate coating: it offers better protection for the metal but is unsuitable as a base for varnish or lacquer.
When oiled, it protects against corrosion. It retains a large quantity of lubricant: its good lubricating properties are useful on sliding machine parts. It is often used for machine, weapon and ammunition components.
- dark grey to black appearance;
- excellent base for retaining lubricating oils;
- recommended when the part heats up in service;
- improves the coefficient of friction and sliding performance.
Manganese-phosphated shafts
Phosphated sleeves
Phosphated tubes
Grain refiners for crystalline phosphating
A grain refiner is often useful in manganese or zinc phosphating processes. Manganese phosphating baths provide excellent corrosion protection, but the coatings they produce are often too thick and coarse-grained to meet the tolerances of mechanical parts, particularly before oiling or on parts subject to friction.
Products: iron phosphating and conversion coating
BONDERITE M-FE HP
Degreaser and phosphating agent for high-pressure application
Substrates and methods: Metal surfaces; High pressure (HP) – 20 to 80 bar; 8 to 15 ml/l at the lance outlet – 60 to 90 °C; Applications: Pretreatment before painting of large or bulky parts that cannot be treated in a spray tunnel
BONDERITE M-FE
Combined degreaser and phosphating agent for a 3-stage spray process line
BONDERITE M-NT 40043
Conversion coating based on zirconium salts. Replaces amorphous phosphating (iron phosphating), reducing phosphate use by a factor of 20 to 100. Degreasing and conversion coating can be combined on short lines (with a detergent additive).
Substrates and methods: Steel, zinc plated steel (electrogalvanized steel), galvanized steel, aluminium; immersion or spray, 3- to 5-stage tunnels; 10 to 30 ml/l; 20 to 25 °C for conversion coating alone, 40 to 60 °C for the combined process; Applications: Pretreatment before painting, particularly powder coating: household appliances, metal furniture, agricultural machinery, radiators
Products: zinc phosphating
BONDERITE M-ZN 2722 E6
Nickel-free bi-cation zinc phosphating with nitrite acceleration (formerly Granodine 2722 E-6 M). Crystalline coating of 2 to 2.8 g/m² providing a good key for subsequent coatings. Particularly suitable before cathodic electrocoating
Substrates and methods: Steel, galvanized steel, Zn/Ni-coated steels; Spray (process sequence with grain refinement and passivation); 50 to 55 °C, 60 to 180 s; Applications: Corrosion-protection pretreatment before cathodic electrocoating or organic coating, including assemblies combining steel and hot-dip galvanized steel
BONDERITE M-ZN 45
Crystalline phosphating by dipping before painting (formerly Granodine 45). Microcrystalline coating of zinc and iron phosphates. Provides a key for paint and passivates the surface
Substrates and methods: Ferrous surfaces; Immersion; 4% + 1% M-AD ZN-2, 70 to 85 °C, 6 to 15 min; Applications: Pretreatment before painting of steel parts treated by dipping
For manganese phosphating and grain refiners, please contact us.
See also:
Steel and multimetal pretreatment →
Conversion coating: multimetal and aluminium →
Corrosion protection →
Surface treatment: all ranges →
Need advice?
Tell us about your parts, substrates, soils and equipment: we will recommend a product and method and send you the technical data sheets and safety data sheets or a quotation.