INFO & QUOTE REQUESTS: info@saphonyx.be

BONDERITE

BONDERITE M: metal pretreatment

Phosphating, conversion coating, passivation, anodizing and post-treatments

The BONDERITE M family (Metal pre-treatment) brings together Henkel products that prepare metal surfaces before painting or bonding and protect them against corrosion: zinc, iron or manganese phosphating, conversion coating with or without chromium, post-treatments, activation, anodizing and sealing.

Saphonyx is a Henkel premium distributor for BONDERITE products in the Benelux (Belgium, the Netherlands, Luxembourg): we help you choose the product and the method, conduct trials and provide follow-up support.

BONDERITE M-ZN: zinc phosphating

Zinc phosphating (Zinc phosphate). On the label and in the technical data sheet: ZINC PHOSPHATE, ZINC PHOSPHATE MAKE UP, ZINC PHOSPHATE REPLENISHER.

BONDERITE M-ZN LITHO-2

Pretreatment of galvanized, zinc-plated or cadmium-plated surfaces before painting: removes white rust to ensure adhesion of the finish; ready to use, approximately 15 m² per kg (formerly LITHOFORME N°2)

Apply undiluted with a brush, leave for 10 to 15 min, then rinse thoroughly with water; wear gloves and safety goggles

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ZN 45

Crystalline phosphating by dipping before painting: microcrystalline layer of zinc and iron phosphates (formerly GRANODINE 45)

Ferrous surfaces; immersion, 4% + 1% BONDERITE M-AD ZN-2, 70 to 85 °C, 6 to 15 min

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ZN 220

Microcrystalline zinc phosphating by immersion, intended for subsequent application of a rust-preventive oil, grease or wax (formerly GRANODINE 220)

Cast iron, plain carbon steels and low-alloy steels; 5 to 8 L + 2 L of BONDERITE M-AD CA-1 per 100 L, 65 to 70 °C, 5 to 10 min

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ZN 2722 E6

Nickel-free, nitrite-accelerated bi-cation zinc phosphating; crystalline layer of 2 to 2.8 g/m², suitable for use before cathodic electrocoating (formerly GRANODINE 2722 E-6 M)

Steel, galvanized steel and Zn/Ni-coated steels; spray, 50 to 55 °C, 60 to 180 s

Featured on:

Technical data sheet (PDF) →

BONDERITE M-FE: iron phosphating

Iron phosphating (Iron phosphate). On the label and in the technical data sheet: IRON PHOSPHATE.

BONDERITE M-FE 30 A

Amorphous iron phosphating with a high coating weight. Former name: Novaphos F 30 A.

Pretreatment of ferrous metals before painting, applied by spray with a surfactant-based detergent additive.

Request the technical data sheet →

BONDERITE M-FE 30A

Amorphous phosphating with a high coating weight for ferrous metals, with a detergent additive (formerly NOVAPHOS F 30 A)

Spray tunnel, 10 to 25 ml/l + 1.5 to 3 ml/l of additive, 30 to 55 °C, 90 to 180 s; coating weight of 0.5 to 1 g/m²

Featured on:

Technical data sheet (PDF) →

BONDERITE M-FE F-813

Amorphous phosphating with a high coating weight for ferrous metals, with a detergent additive (formerly DURIDINE F 813 CF)

Spray tunnel, 12 to 25 ml/l + 1.5 to 3 ml/l of additive, 30 to 55 °C, 90 to 180 s

Featured on:

Technical data sheet (PDF) →

BONDERITE M-FE F-814

Single-step degreasing and amorphous phosphating of steel, usable at temperatures as low as 25 °C (formerly DURIDINE F 814 CF)

Three- or four-stage spray tunnel; 2% at 35–40 °C for 3 min, up to 4% for 1 min

Featured on:

Technical data sheet (PDF) →

BONDERITE M-FE 1070

Multimetal degreasing and phosphating: steel, light alloys, galvanized steel, zinc plated steel (formerly DURIDINE 1070)

Spray for 90 s to 3 min or immerse for 3 to 8 min; 3 to 6% by volume, 40 to 65 °C

Featured on:

Technical data sheet (PDF) →

BONDERITE M-FE HP

Iron phosphate degreaser and phosphating agent for high-pressure equipment (formerly NOVAPHOS F HP): degreasing and phosphating in a single operation

For bulky parts that cannot be treated in a tunnel; 8 to 15 ml/l at the lance outlet, 60 to 90 °C, 20 to 80 bar; remove rust from rusty parts before treatment

Featured on:

Technical data sheet (PDF) →

BONDERITE M-MN: manganese phosphating

Manganese phosphating (Manganese phosphate). On the label and in the technical data sheet: MANGANESE PHOSPHATE.

BONDERITE M-MN 2252

Manganese phosphating of steel and cast iron friction components; a single product for bath make-up and maintenance (formerly NOVAPHOS M 2252)

Immersion (barrel, basket or rack), 80 to 100 L per 1,000 L, 95 to 98 °C, 5 to 15 min

Featured on:

Technical data sheet (PDF) →

BONDERITE M-CR: chromating (chromate conversion coating)

Chromating (chromate conversion coating) (Chromating). On the label and in the technical data sheet: CHROMATE COATING.

BONDERITE M-CR 871

No-rinse, hexavalent chromium-free conversion coating (formerly ALODINE 871 TOUCH-N-PREP). Stick applicator for touch-ups

Aluminium and its alloys; apply manually with the stick and allow to air-dry — Touch-ups on damaged surfaces: corrosion protection and a base for paint adhesion or adhesive bonding

Featured on:

Technical data sheet in English (PDF) →

BONDERITE M-CR 871 AERO

No-rinse, hexavalent chromium-free conversion coating (formerly ALODINE 871 TOUCH-N-PREP). Stick applicator for touch-ups

Substrates and methods: Aluminium and its alloys; manual application with the stick, air drying; applications: Touch-ups on damaged surfaces: corrosion protection and an adhesion-promoting base for painting or bonding

Featured on:

Technical data sheet in English (PDF) →

BONDERITE M-CR 1132 AERO

No-rinse chromate conversion coating (hexavalent chromium) in a stick applicator for touch-ups (formerly ALODINE 1132 TOUCH-N-PREP)

Apply with the stick in two passes at right angles and allow to air-dry; for aluminium, ferrous metals and galvanized steel; classes 1A and 3 (MIL-DTL-81706)

Featured on:

Technical data sheet (PDF) →

BONDERITE M-CR 1200 AERO

Powdered chromate conversion coating for aluminium (formerly ALODINE 1200). Golden yellow to brown coating, with virtually no dimensional build-up. Approved to MIL-C-5541, QPL 81706 list

Substrates and methods: Aluminium and light alloys; Immersion; 15 g/l, 20 to 40 °C, 45 s to 3 min; Applications: Long-lasting corrosion protection of unpainted or locally painted parts; pretreatment before painting

Featured on:

Technical data sheet (PDF) →

BONDERITE M-CR 1200S

Powdered chromate conversion coating for aluminium (formerly ALODINE 1200 S). Class 1A and Class 3 coatings to MIL-DTL-5541 (QPL-81706), painted or unpainted. Contains hexavalent chromium: chromium trioxide under REACH authorisation

Substrates and methods: Aluminium and light alloys; Immersion – Spray – Brush; 7.5 g/l (brush 15 g/l), 20 to 35 °C, 15 s to 3 min; Applications: Corrosion protection of aluminium and base for paint adhesion

Featured on:

Technical data sheet (PDF) →

BONDERITE M-CR 1500 AERO

Colourless liquid chromate conversion coating (formerly ALODINE 1500). Retains the appearance of the metal; does not interfere with spot welding. Class 3 coatings to MIL-DTL-5541 (QPL MIL-DTL-81706)

Substrates and methods: Aluminium and light alloys; Immersion – Spray; 1% vol., 60 to 70 °C; immersion 2 to 5 min, spray 15 s to 2 min; Applications: Corrosion protection and base for adhesion of clear lacquers or paints, where the appearance of the aluminium must be retained

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT: new-generation conversion coatings, usually chrome-free; combined degreasers and conversion coatings

New-generation conversion coatings, usually chrome-free; combined degreasers and conversion coatings (New technology). On the label and in the technical data sheet: CONVERSION COATING, CR FREE CONVERSION COATING, CLEANER / COATER.

BONDERITE M-NT 1

Phosphate-free “nanoceramic” conversion coating (formerly BONDERITE NT 1). Designed to replace amorphous phosphating; eliminates the passivation stage. Operates at room temperature

Substrates and methods: Steel, zinc plated steel (electrogalvanized steel), galvanized steel, aluminium; immersion or spray; 30 to 50 ml/l, 20 to 30 °C, 20 to 120 s; Applications: Pretreatment before painting, particularly powder coating

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 160 / M-NT 161

Chrome-free conversion coating containing neither trivalent nor hexavalent chromium (formerly ALODINE 160 / 161). Yellow coating visible to the naked eye. Free from heavy metals and organic compounds

Substrates and methods: Aluminium, magnesium and their alloys, including casting alloys; immersion; 5 to 20 g/l (160) + 6 to 24 g/l (161), 20 to 30 °C, 30 to 180 s; Applications: Paint adhesion and corrosion protection in construction, automotive, electronics and industrial applications

Featured on:

Request the technical data sheet →

BONDERITE M-NT 400

Chrome-free conversion coating for aluminium and its alloys. Former name: ALODINE 400.

Provides a base for paint adhesion and corrosion protection for painted parts; applied by immersion or spray; also used for final passivation after phosphating.

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 1200

Spray-applied phosphate-free conversion coating (formerly TECTALIS 1200). Designed to replace crystalline zinc phosphating. Eliminates the grain-refining and passivation stages

Substrates and methods: Steel, electrogalvanized steel, galvanized steel, aluminium; spray application in existing installations; 30 g/l at bath make-up, 20 to 40 °C, 20 to 180 s; Applications: Before all types of paint, particularly cathodic electrocoating and powder coating: automotive, agricultural machinery, household appliances and metal furniture

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 1455 WIPES

Pre-impregnated wipes for chrome-free conversion coating (formerly GRANODINE 1455 WIPES). Treatment of small areas without disassembly or rinsing

Substrates and methods: Aluminium, zinc and their alloys, steel, electrogalvanized steel and galvanized steel; dabbing or wiping; undiluted, 20 to 30 °C, 30 to 60 s; Applications: Touch-ups and repairs before painting, varnishing or bonding

Featured on:

Request the technical data sheet →

BONDERITE M-NT 1455T

Chrome-free passivation after phosphating (formerly GRANODINE 1455 T). After amorphous or crystalline zinc phosphating. Complies with the ELV and RoHS directives

Substrates and methods: Steel, galvanized steel, electrogalvanized steel, aluminium; Immersion – Spray; 2 to 10 ml/l (generally 5 ml/l), 20 to 40 °C, 20 to 60 s; Applications: Post-treatment before cathodic electrodeposition, liquid or powder paints

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 1800

Phosphate-free pretreatment for multimetal substrates with a high proportion of aluminium. An alternative to zinc phosphating with fewer treatment stages. Free from regulated heavy metals, with no biochemical oxygen demand (BOD) or chemical oxygen demand (COD)

Substrates and methods: Multimetal substrates, including those with a high proportion of aluminium; operates at room temperature; Applications: Vehicle bodies and automotive components with a high proportion of aluminium

Featured on:

Request the technical data sheet →

BONDERITE M-NT 2040 R2

Chrome-free conversion coating for aluminium with a self-regulating coating weight. Short 5-stage process: combined pickling and degreasing followed by conversion coating, without an intermediate rinse. Can also directly replace an existing chromate conversion process.

Substrates and methods: Aluminium profiles and sheets; immersion; example: 2% bath with a degreasing additive, followed by a 1% bath, 30 s to 1 min at room temperature; Applications: Pretreatment of architectural aluminium before powder coating, with fewer stages and less water

Featured on:

Request the technical data sheet →

BONDERITE M-NT 2040 R9

Chrome-free deoxidation and passivation of aluminium. The same product is used for the deoxidation bath and the conversion coating bath, with M-AD 338. Stabilises surface resistivity by limiting reoxidation

Substrates and methods: Aluminium; immersion – spray; conversion coating: 10 ml/l (+ 0.3 ml/l M-AD 338), 25 to 50 °C, 25 s to 1 min 30 s; Applications: Pretreatment of aluminium before painting, bonding or welding

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 4830 / M-NT 4831

Two-component chrome-free conversion coating, with or without a final rinse (formerly ALODINE 4830 / 4831)

Immersion, spray or cascade; 2 to 5 ml/l (4830) + 7 to 12 ml/l (4831), 15 to 40 °C, 15 to 60 s; approved by Qualicoat and GSB

Featured on:

Request the technical data sheet →

BONDERITE M-NT 4850-2

Chrome-free conversion coating (neither hexavalent nor trivalent chromium), with a single product for bath make-up and maintenance (formerly ALODINE 4850-2)

Aluminium and its alloys, including casting alloys; immersion or spray, 5 to 20 ml/l, 20 to 40 °C, 30 to 90 s; approved by Qualicoat and GSB

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 5700 AERO

Ready-to-use chrome-free conversion coating (formerly ALODINE 5700). Can be dried at 20 to 100 °C without loss of corrosion resistance. Can be used without rinsing, depending on the conditions of use

Substrates and methods: Aluminium and its alloys; spray application, undiluted; room temperature (preferably 20 to 25 °C), contact time of 1 to 5 min; Applications: Pretreatment before painting during the repair and repainting of aircraft and aluminium parts

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 5700 AERO WIPES

Pre-impregnated wipes for chrome-free conversion coating (formerly ALODINE 5700 WIPES). Treatment of small areas without disassembly or rinsing

Substrates and methods: Aluminium, titanium, magnesium; dabbing or wiping; undiluted, 20 to 30 °C, 30 to 60 s; Applications: Aerospace repairs and repainting: promotes adhesion of paints, varnishes or adhesives

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 5992

Hexavalent chromium-free conversion coating for aluminium (formerly ALODINE 5992). Mineral base: trivalent chromium and zirconium salts. Meets QUALICOAT requirements (polyester powder coating)

Substrates and methods: Aluminium and its alloys, including casting alloys; hot-dip galvanized steel; spray or immersion (immersion for galvanized steel); Aluminium: 30 to 60 ml/l, 25 to 35 °C, 30 to 90 s; Applications: Base for paint adhesion on aluminium; protection of hot-dip galvanized parts, painted or unpainted

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 20120

Conversion coating free of phosphates, VOCs and toxic heavy metals. Generally provides better corrosion protection than iron phosphating with a chrome-free final rinse. Limits “flash rust” during line stoppages

Substrates and methods: Steel, galvanized steel, aluminium; spray or immersion, without heating; 1 to 3.5%, 20 to 50 °C, 20 to 120 s; Applications: Pretreatment before painting, compatible with all types of paint

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 30002

Phosphate-free multimetal conversion coating based on trivalent chromium and zirconium. Particularly suitable for zinc-coated substrates. Requires no heating; limits “flash rust” during short line stoppages

Substrates and methods: Steel, galvanized steel, aluminium; spray or immersion; 3% at bath make-up, 20 to 35 °C, 30 to 120 s; Applications: Pretreatment before applying any type of paint, for example on agricultural equipment

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 40043

Conversion coating based on zirconium salts. Replaces amorphous phosphating (iron phosphating), reducing phosphate use by a factor of 20 to 100. Degreasing and conversion coating can be combined on short lines (with a detergent additive).

Substrates and methods: Steel, zinc plated steel (electrogalvanized steel), galvanized steel, aluminium; immersion or spray, 3- to 5-stage tunnels; 10 to 30 ml/l; 20 to 25 °C for conversion coating alone, 40 to 60 °C for the combined process; Applications: Pretreatment before painting, particularly powder coating: household appliances, metal furniture, agricultural machinery, radiators

Featured on:

Technical data sheet (PDF) →

BONDERITE M-NT 50001

No-rinse thin-film conversion coating (APNR process) for lines with fewer than 5 stages

Steel, galvanized steel, aluminium; spray application after degreasing using the APNR equipment, 0.2 to 1%, room temperature, 5 to 60 s

Featured on:

Technical data sheet in English (PDF) →

BONDERITE M-NT 65000 AERO

Trivalent chromium and zirconium conversion coating for aluminium (formerly ALODINE 5923 PLUS), free of hexavalent chromium: corrosion protection for bare metal, paint adhesion, low electrical contact resistance; approved to MIL-DTL-81706

Concentrated liquid; immersion without agitation or brush application; colourless to iridescent coating that can be inspected with the BONDERITE Viewer

Featured on:

Request the technical data sheet →

BONDERITE M-NT E

Chrome-free conversion coating requiring infrequent bath replacement, resulting in a low volume of effluent (formerly ALODINE NTE)

Aluminium, electrogalvanized steel and galvanized steel; 5% M-NT E + 0.2% M-NT 4830, 20 to 30 °C, 30 to 90 s; approved by Qualicoat

Featured on:

Technical data sheet (PDF) →

BONDERITE M-PT: post-treatment after phosphating or conversion coating, with or without chromium

Post-treatment after phosphating or conversion coating, with or without chromium (Post treatment). On the label and in the technical data sheet: POST TREATMENT, CR FREE POST TREATMENT, TRI CHROME POST TREATMENT, HYDROPHILIC COATING.

BONDERITE M-PT 54 NC

Chrome-free inorganic passivation, acid post-rinse (formerly DEOXYLYTE 54 NC). For zinc and iron phosphate coatings. Improves corrosion protection and paint adhesion

Substrates and methods: Phosphated surfaces (zinc or iron phosphate); Spray – Immersion; 2.5 ml/l, pH 4 to 4.5 (adjusted with M-AD 80L), 20 to 55 °C, 15 to 90 s; Applications: Post-rinse after phosphating, before all paint systems

Featured on:

Technical data sheet (PDF) →

BONDERITE M-PT 98 NC

Chrome-free passivation after amorphous phosphating (formerly DEOXYLYTE 98 NC). Reinforces the corrosion protection of the coating and paint adhesion

Substrates and methods: Steel, galvanized steel, electrogalvanized steel, aluminium; Immersion – Spray; 0.5 to 2 ml/l (0.2 to 1 ml/l in deionized water), 20 to 40 °C, 20 to 60 s; Applications: Post-treatment on amorphous phosphating lines, before cathodic electrodeposition, liquid or powder paint

Featured on:

Technical data sheet (PDF) →

BONDERITE M-PP: painting processes

Painting processes: autodeposition (Paint process). On the label and in the technical data sheet: AUTODEPOSITION COATING.

BONDERITE M-PP 866 R

Black organic coating applied by autodeposition to ferrous parts, with a low curing temperature (formerly AQUENCE 866)

Immersion in a bath at 20-22 °C; oven curing at around 90 °C; withstands temperatures up to 100 °C

Featured on:

Technical data sheet in English (PDF) →

BONDERITE M-PP 930 MU / M-PP 930 R

Black organic coating applied by autodeposition to ferrous parts, compatible with powder coating (formerly AQUENCE 930)

Immersion in a bath at 20-22 °C; oven curing at around 175 °C; withstands temperatures above 220 °C

Featured on:

Request the technical data sheet →

BONDERITE M-AC: activation and grain refinement before phosphating

Activation and grain refinement before phosphating (Activator / Surface conditioner). On the label and in the technical data sheet: PHOSPHATE ACTIVATOR.

BONDERITE M-AC TG-2 / M-AC TG-2 B

Two-component grain refiner for use before manganese phosphating: a fine, homogeneous layer with a uniform black appearance (formerly FIXODINE TG 2A / TG 2B)

Essential after strongly alkaline degreasing or acid pickling

Featured on:

Request the technical data sheet →

BONDERITE M-AC 50 CF

Grain refiner for use before crystalline zinc phosphating, suitable for bath make-up with industrial water (formerly FIXODINE 50 CF)

By immersion or in the second rinse after degreasing, immediately before phosphating

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ED: electrodeposition

Electrodeposition: anodizing, sealing, electrodeposited coatings (Electro deposition). On the label and in the technical data sheet: ANODIZING, ANODIZING SEAL, ELECTRODEPOSITION COATING.

BONDERITE M-ED ECC 9000

Electrolyte for the BONDERITE ECC electroceramic coating. Oxide layer deposited by micro-arcs (plasma), with hardness comparable to that achieved by hard anodizing. Heavy metal-free electrolyte, compatible with REACh and RoHS

Substrates and methods: Aluminium and its alloys (including casting alloys), titanium and its alloys; immersion with pulsed current, with the workpiece as the anode; Applications: Corrosion protection, hardness and paint adhesion: marine applications, outdoor lighting, engines, electronics; alternative to chromic acid anodizing or hard anodizing

Featured on:

Request the technical data sheet →

BONDERITE M-ED 11006

Anti-smut additive for hot sealing (> 96 °C) of anodized aluminium (formerly P3-ALMECO SEAL QUICK)

1 to 2 g/l (clear) or 2 to 3 g/l (coloured) in deionized water, pH 5.5 to 6.5; sealing time: 2 min/µm

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ED 11100

Cold sealing by impregnation (nickel fluoride) after clear or coloured anodizing (formerly ALMECO SEAL 11100)

Immersion, 4 to 6 g/l, 23 to 28 °C, pH 5.8 to 6.5, 0.7 to 1.2 min per µm of oxide

Featured on:

Technical data sheet (PDF) →

BONDERITE M-ED 12003

Additive for tin(II) electrolytic colouring baths: stability and throwing power (formerly ALMECO COLOR S)

20 to 25 g/l with 8 to 10 g/l tin and 18 to 22 g/l sulphuric acid, 18 to 24 °C, 30 s to 15 min depending on the shade

Featured on:

Technical data sheet (PDF) →

BONDERITE M-AD: additives

Additives: phosphating accelerators and additives for pretreatment, anodizing and autodeposition (Additives). On the label and in the technical data sheet: PHOSPHATE ACCELERATOR, PRETREATMENT ADDITIVE, ANODIZING ADDITIVE.

BONDERITE M-AD 80L

Weakly alkaline pH adjuster (inorganic salt in solution) used to neutralise acidic facade cleaning products

Use neat for the first rinse; add to the rinse water where plants are present

Featured on:

Technical data sheet in English (PDF) →

BONDERITE M-AD 2000A

Additive for sulphuric acid anodizing baths that reduces redissolution of the oxide layer (formerly ALMECO OX 2000 A)

15 to 30 ml/l in 180 to 220 g/l sulphuric acid, 18 to 24 °C, 1.2 to 4 A/dm²

Featured on:

Technical data sheet (PDF) →

Other codes in the family

M-PA (passivation). None of these products is featured on our site yet: ask us for advice.

The BONDERITE families

The whole BONDERITE brand: codes, families and former names →

Find a former name

Henkel products formerly sold under the names ALODINE, GRANODINE, P3, RIDOLINE or TURCO now carry the BONDERITE name.

Correspondence table: nearly 2,500 former names →
TURCO name conversion: some 270 former TURCO products →

Need advice?

Can’t find your product? The BONDERITE range is wider than the products featured here. Tell us about your parts, substrates, soils and equipment: we will recommend the product and the method, and send you the technical data sheets and safety data sheets or a quotation.